Analysis of mAb stability by Differential scanning calorimetry (DSC) (CAT#: STEM-MB-0497-WXH)

Introduction

mAb has offered promising potential applications as drugs in the pharmaceutical industry. Being a therapeutic agent, antibodies must be in the native, monomeric state to have a proper function with good stability. It is also essential to minimize the aggregation of antibodies for pharmaceutical applications. Previously, it has been confirmed that at the time of purification and viral clearance, the acidic environment induces conformational changes in antibodies, particularly in their Fc domain. Hence, the importance of understanding such conformational changes, together with the stability and aggregation of antibodies at different pH values, comes into the picture.

STEMart technology detail



Principle

Calorimetry is a primary technique for measuring the thermal properties of materials to establish a connection between temperature and specific physical properties of substances and is the only method for direct determination of the enthalpy associated with the process of interest. Calorimeters are used frequently in chemistry, biochemistry, cell biology, biotechnology, pharmacology, and recently, in nanoscience to measure thermodynamic properties of the biomolecules and nano-sized materials.
Amongst various types of calorimeters, differential scanning calorimeter (DSC) is a popular one. DSC is a thermal analysis apparatus measuring how physical properties of a sample change, along with temperature against time.1In other words, the device is a thermal analysis instrument that determines the temperature and heat flow associated with material transitions as a function of time and temperature. During a change in temperature, DSC measures a heat quantity, which is radiated or absorbed excessively by the sample on the basis of a temperature difference between the sample and the reference material.

Applications

Analysis of mAb stability
Drug discovery in the pharmaceutical industry

Procedure

1. Instrument Start-up
2. Sample Preparation
(1) Dialyze the sample against the buffer that will be used as the reference for the experiment.
(2) Determine the concentration of the protein sample using the most suitable protein concentration determination method.
(3) Degas the sample and reference buffer in vacuum to get rid of microbubbles that can cause volume inaccuracy.
(4) load the samples and their respective buffer in pairs into 96 well plates compatible with the instrument.
(5) Place the plate in the sample holding compartment in the proper orientation.
3. Experimental Parameter Setup
Set the starting temperature, final temperature and the scan rate of the experiment.
4. Data Analysis

Materials

Differential Scanning Calorimeters
High-quality products

High-quality products

Reliable performance

Wide range of applications

Wide range of applications

For various laboratory needs

Expert support

Expert support

Professional service team

Fast delivery

Fast delivery

Global shipping